Key Attributes
  • Excellent thermal stability
  • High softening point
  • Made from purified aromatic monomers
  • Water-white initial color

Product Description
Kristalex™ F115 hydrocarbon resin is a water-white, color stable, low molecular weight thermoplastic hydrocarbon polymer. Based on purified 8-9 carbon aromatic monomers, this resin is indicated for use in plastics modification, hot melt adhesives and coatings, sealants and caulks. Kristalex F115 is compatible with a wide variety of oils, waxes, alkyds, plastics, and elastomers, and is soluble in many common organic solvents.











In EVA-based hot melt adhesives Kristalex F115 has useful compatibility with EVA grades with up to 30% vinyl acetate and is useful in formulating low-color adhesives with improved high temperature resistance. In styrenic block copolymer based adhesives Kristalex F115 preferentially associates with the styrenic endblocks, producing higher cohesion at temperatures up to 70°C without affecting tack and adhesion properties.


Typical Properties

PropertyTest MethodTypical Value, Units
General
Ring and Ball Softening PointASTM E 28117 °C
Colora 
     Hunterlab b, 5 cm path lengthASTM E 3132
Bromine Number 7 g/100g
Density 
     @ 25°C 1.06 kg/dm3
Cloud Pointb 
     OMS 110
Molecular Weightc 
     Mn 980
     Mw 1850
     Mw/Mn 1.6
     Mz 3180
Melt Viscosity 
     @ 140°C 46000 cP
     @ 160°C 5500 cP
     @ 180°C 1200 cP
     @ 200°C 400 cP

a50% solids in toluene, 50 mm path length, Illuminant C, and a 2° observer.
bCloud point temperature testing by Eastman methods. OMS from odorless mineral spirits.
cMolecular weight measured via Gel Permeation Chromatography (GPC) using polystyrene standards, elution with THF.



Compatibility and Solubility
Compatible at all ratios, or in limited but practically useful proportions, with a wide variety of materials such as styrene-butadiene rubber (SBR) and SBR block copolymers, neoprene, nitrile, polybutadiene, acrylic polymers, chlorinated rubber, EVA resins (ethylene-vinyl acetate copolymers), styrenated alkyds, vinylated alkyds, drying oil alkyds, rosin ester resins, as well as modifying the styrenic endblocks of all styrene-containing block copolymers.

Soluble in aromatic and chlorinated hydrocarbons, esters, and ketones. Insoluble in aliphatic hydrocarbons; alcohols and glycols. Limited solubility in nitroparaffins.

Packaging
Kristalex™ F115 hydrocarbon resin is pastillated and packed in polyethylene bags of 25 kg net, and supplied on shrink-wrapped pallets of 40 bags (1000 kg) each, from Eastman facilities in the Netherlands and from warehouses located in Europe.

Storage
Due to the thermoplastic behavior, pastillated and flaked resins may fuse, block or lump. This can be accelerated under any of the following conditions: 1) above ambient temperature 2) prolonged storage 3) pressure, e.g., stacking pallets, or a combination of these conditions. This is particularly applicable for low softening point resin grades. In order to maintain the flake or pastille shape, we therefore recommend storing the material in a temperature-controlled area, be careful with stacking material or applying pressure and preventing prolonged storage. It should be noted that lumping does not have a negative impact on the product specifications. Due to the nature of the product, claims regarding lumping cannot be accepted.





Resins are prone to gradual oxidation, some more so than others. This could result in darkening and/or it could have an adverse effect on the solubility of the resin in organic solvents or on its compatibility with polymers. Accordingly, it is recommended that strict control of inventory be observed at all times, taking care that the oldest material is used first.





Kristalex™ F115 hydrocarbon resin material will remain within product specification limits, as mentioned under the heading "Product Specifications" (overleaf), for a period of at least twelve months after shipment from Eastman production facilities in the Netherlands, provided storage conditions outlined in this data sheet are observed. However, as we can neither anticipate the conditions under which the resin is processed nor the end use applications for which it is used, we recommend that the material be tested upon receipt.

Comments
Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.


Eastman and its marketing affiliates shall not be responsible for the use of this information, or of any product, method, or apparatus mentioned, and you must make your own determination of its suitability and completeness for your own use, for the protection of the environment, and for the health and safety of your employees and purchasers of your products. No warranty is made of the merchantability of fitness of any product, and nothing herein waives any of the Seller's conditions of sale.