Propertya | Test Methodb | Typical Value, Unitsc |
|
Electrical Properties (ASTM Method) |
Dielectric Constant | |
1 kHz | D 150 | 2.3 |
1 MHz | D 150 | 2.1 |
Dissipation Factor | | 1 kHz | D 150 | 0.002 |
1 MHz | D 150 | 0.008 |
Arc Resistance | D 495 | 143 sec |
Volume Resistivity | D 257 | 1015 ohm·cm |
Surface Resistivity | D 257 | 1016 ohms/square |
Dielectric Strength, Short Time, 500 V/sec rate-of-rise | D 149 | 17.3 kV/mm (440 V/mil) |
Comparative Tracking Index | D 3638 | >600 V |
Electrical Properties (UL Method) |
|
High Voltage Arc Tracking Resistance | UL 746A | 38 mm/min (1.5 in./min) |
General Properties (ASTM Method) |
|
Specific Gravity | D 792 | 1.20 |
Water Absorption, 24 h immersion | D 570 | 0.13 % |
Mold Shrinkage | | Parallel to Flow, 3.2-mm (0.125-in.) thickness | D 955 | 0.005-0.007 mm/mm (0.005-0.007 in./in.) |
General Properties (ISO Method) |
|
Density | ISO 1183 | 1.20 g/cm3 |
Water Absorption, 24 h immersion | ISO 62 | 0.13 % |
Mechanical Properties (ASTM Method) |
|
Tensile Stress @ Yield | D 638 | 56 MPa (8100 psi) |
Tensile Stress @ Break | D 638 | 60 MPa (8700 psi) |
Elongation @ Yield | D 638 | 6 % |
Elongation @ Break | D 638 | 150 % |
Flexural Modulus | D 790 | 2140 MPa (3.1 x 105 psi) |
Flexural Yield Strength | D 790 | 86 MPa (12500 psi) |
Rockwell Hardness, R Scale | D 785 | 117 |
Izod Impact Strength, Notched | | @ 23°C (73°F) | D 256 | NB |
@ -40°C (-40°F) | D 256 | 75 J/m (1.4 ft·lbf/in.) |
Impact Strength, Unnotched | | @ 23°C (73°F) | D 4812 | NB |
@ -40°C (-40°F) | D 4812 | NB |
Impact Resistance (Puncture), Energy @ Max. Load | | @ 23°C (73°F) | D 3763 | 51 J (38 ft·lbf) |
@ -40°C (-40°F) | D 3763 | 46 J (34 ft·lbf) |
Mechanical Properties (ISO Method) |
|
Tensile Stress @ Yield | ISO 527 | 56 MPa |
Tensile Stress @ Break | ISO 527 | 56 MPa |
Elongation @ Yield | ISO 527 | 5.4 % |
Elongation @ Break | ISO 527 | 130 % |
Flexural Modulus | ISO 178 | 2100 MPa |
Flexural Yield Strength | ISO 178 | 81 MPa |
Izod Impact Strength, Notched | | @ 23°C | ISO 180 | 10 kJ/m2 |
@ -40°C | ISO 180 | 8.3 kJ/m2 |
Impact Resistance (Puncture), Energy @ Max. Load | | @ 23°C | ISO 6603-2 | 19 J |
@ -40°C | ISO 6603-2 | 23 J |
Optical Properties (ASTM Method) |
|
Haze | D 1003 | 3.6 % |
Regular Transmittance | D 1003 | 77 % |
Total Transmittance | D 1003 | 81 % |
Thermal Properties (ASTM Method) |
Deflection Temperature | |
@ 0.455 MPa (66 psi) | D 648 | 103 °C (218 °F) |
@ 1.82 MPa (264 psi) | D 648 | 90 °C (194 °F) |
Vicat Softening Temperature | | @ 1 kg load | D 1525 | 118 °C (244 °F) |
Specific Heat | | @ 240°C (464°F) | DSC | 2.18 kJ/kg·K (0.52 Btu/lb·°F) |
@ 60°C (140°F) | DSC | 1.38 kJ/kg·K (0.33 Btu/lb·°F) |
Thermal Properties (ISO Method) |
Deflection Temperature | |
@ 0.45 MPa | ISO 75 | 103 °C |
@ 1.80 MPa | ISO 75 | 90 °C |
Vicat Softening Temperature | | @ 1 kg load | ISO 306 | 118 °C |
@ 5 kg load | ISO 306 | 110 °C |
Thermal Properties (UL Method) |
UL Flammability Classificationd | |
1.6 mm (0.0625 in.) specimen | UL 94 | 94HB |
3.2 mm (0.125 in.) specimen | UL 94 | 94V-2 |
Typical Processing Conditions |
|
Drying Temperature | | 93 °C (200 °F) |
Drying Time | | 4-6 hrs |
Processing Melt Temperature | | 271-293 °C (520-560 °F) |
Mold Temperature | | 32-66 °C (90-150 °F) |
|