Technical Data Sheet
Eastman Tritan™ Copolyester TX1001
Applications
Appliances (food contact)
Compounders
Consumer electronics
Consumer housewares - food contact (FC)
Consumer housewares-NFC
Displays/in-store fixtures
Electronic packaging
Equipment & machinery
Filtration
Industrial
Large appliances non-food contact
Lighting
Non-kitchen appliances
Non-medical housings & hardware for elec
Outdoor signs
Packaging components non food contact
Packaging tape
Personal care & cosmetics packaging
Personal care bottles
Personal care packaging
Point-of-purchase
Protective & performance film
Small appliances non-food contact
Sporting equipment
Tools
Toys
Water/sport bottles
Key Attributes
Ease of processing
Excellent clarity
Excellent hydrolytic stability
Fast drying times
Good chemical resistance
Good heat resistance
Outstanding impact resistance
Quick cycle times
Product Description
Eastman Tritan™ TX1001 is an amorphous copolyester with excellent appearance and clarity. Tritan TX1001 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity and aggressive cleaning detergents. Tritan TX1001 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Tritan TX1001 is certified to NSF/ANSI Standard 51 for Food Equipment Materials and is also certified to NSF/ANSI/CAN Standard 61 – Drinking Water System Components-Health Effects.
Typical Properties
Property
a
Test Method
b
Typical Value, Units
c
General Properties
Specific Gravity
D 792
1.18
Mold Shrinkage
D 955
0.005-0.007 mm/mm (0.005-0.007 in./in.)
Mechanical Properties (ISO Method)
Tensile Stress @ Yield
ISO 527
43 MPa
Tensile Strength @ Break
ISO 527
58 MPa
Elongation @ Yield
ISO 527
7 %
Elongation @ Break
ISO 527
185 %
Tensile Modulus
ISO 527
1548 MPa
Flexural Modulus
ISO 178
1495 MPa
Flexural Strength
ISO 178
59 MPa
Izod Impact Strength, Notched
@ 23°C
ISO 180
93 kJ/m
2
@ -40°C
ISO 180
20 kJ/m
2
Mechanical Properties
Tensile Stress @ Yield
D 638
43 MPa (6200 psi)
Tensile Stress @ Break
D 638
53 MPa (7700 psi)
Elongation @ Yield
D 638
6 %
Elongation @ Break
D 638
210 %
Tensile Modulus
D 638
1550 MPa (2.25 x 10
5
psi)
Flexural Modulus
D 790
1550 MPa (2.25 x 10
5
psi)
Flexural Yield Strength
D 790
62 MPa (9000 psi)
Rockwell Hardness, R Scale
D 785
112
Izod Impact Strength, Notched
@ 23°C (73°F)
D 256
980 J/m (18.4 ft·lbf/in.)
Impact Strength, Unnotched
@ 23°C (73°F)
D 4812
NB
Optical Properties
Total Transmittance
D 1003
90 %
Haze
D 1003
<1 %
Thermal Properties
Deflection Temperature
@ 0.455 MPa (66 psi)
D 648
99 °C (210 °F)
@ 1.82 MPa (264 psi)
D 648
85 °C (185 °F)
Typical Processing Conditions
Drying Temperature
88 °C (190 °F)
Drying Time
4-6 hrs
Processing Melt Temperature
260-282 °C (500-540 °F)
Mold Temperature
38-66 °C (100-150 °F)
a
Unless noted otherwise, all tests are run at 23°C (73°F) and 50% relative humidity.
b
Unless noted otherwise, the test method is ASTM.
c
Units are in SI or US customary units.
Technical Disclaimer
Eastman makes no representation and disclaims any warranty that the material in any particular shipment will conform exactly to the values given. Values as well as the performance of the final molded article may be affected by various factors such as the part design, mold design or tooling, drying, processing conditions as well as coloring or pigmentation of the product. No warranty of merchantability or fitness for use is made, and nothing herein waives any of the Seller''''''''''''''''s conditions of sale. You must make your own determination of the suitability of this product in your specific application due to the many factors (e.g. design, processing and conditions of use) that affect the performance of the final molded article. Suitability of use should be evaluated with appropriate testing and analysis. The processing melt temperature and mold temperature refer to the actual resin melt temperature and actual mold surface temperature respectively. Consider overall resin residence time, part shot size utilization and part geometry to set appropriate processing melt temperature and mold temperature in order to minimize IV loss and maximize molded part performance.
Comments
Properties reported here are based on limited testing. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.
Eastman and its marketing affiliates shall not be responsible for the use of this information, or of any product, method, or apparatus mentioned, and you must make your own determination of its suitability and completeness for your own use, for the protection of the environment, and for the health and safety of your employees and purchasers of your products. No warranty is made of the merchantability of fitness of any product, and nothing herein waives any of the Seller's conditions of sale.
8/21/2024 9:07:18 AM