Click for PDF View TDS
Technical Data Sheet
Eastman Cadence™ Copolyester GS5


Applications
  • Decorative laminates-cabinetry
  • Decorative laminates-wood
  • Flooring
  • Labels non food contact
  • Shrink film non food contact
  • Transaction cards
  • Wallpaper
  • Walls
  • Wood furniture

Product Description
Eastman Cadence™ GS5 is an amorphous copolyester with improved processability for film calendering. Calendered films made of Eastman Cadence™ copolyester are non-crystallizing, are halogen-free, offer wide calendering and thermoforming windows and have good low-temperature toughness. They are cooperative in secondary operations such as solvent-bonding, lamination, decoration, cold-forming, punching/cutting and embossment.

Eastman Cadence™ resins require no pre-drying or additional stabilizers.

This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.
The GREENGUARD INDOOR AIR QUALITY CERTIFIED® Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products.

This product has been CRADLE TO CRADLE CERTIFIEDTM Bronze, with Material Health Certificate, Platinum.
The CRADLE TO CRADLE CERTIFIED mark is a registered certification mark used under license through the Cradle to Cradle Products Innovation Institute, a nonprofit organization that administers the publicly available Cradle to Cradle CertifiedTM Product Standard which provides designers and manufacturers with criteria and requirements for continually improving product materials and manufacturing processes. The Cradle to Cradle CertifiedTM Product Standard guides designers and manufacturers through a continual improvement process that looks at a product through five quality categories—material health, material reutilization, renewable energy and carbon management, water stewardship, and social fairness. A product receives an achievement level in each category—Basic, Bronze, Silver, Gold, or Platinum—with the lowest achievement level representing the product’s overall mark.

The Material Health Certificate provides manufacturers with a trusted way to communicate their efforts to identify and replace chemicals of concern in their products. For more information about Cradle to Cradle certification and to obtain printable certificates for Eastman copolyesters, visit www.c2ccertified.org. Search for Eastman Chemical Company in Cradle to Cradle Certified Products Registry.



Typical Properties

PropertyaTest MethodbTypical Value, Unitsc
Calender Film: Clear (Unpigmented)
Specific GravityD 7921.27
Tensile Strength @ Break 
     M.D.D 88250 MPa (7200 psi)
     T.D.D 88248 MPa (7000 psi)
Tensile Modulus, Tangent 
     M.D.D 8821870 MPa (2.7 x 105 psi)
     T.D.D 8821825 MPa (2.6 x 105 psi)
Tensile Modulus, 1% Secant 
     M.D.D 8821800 MPa (2.6 x 105 psi)
     T.D.D 8821760 MPa (2.6 x 105 psi)
Brittleness Temperature by ImpactdD 1790-45 °C (-49 °F)
Durometer Hardness 
     Shore A ScaleD 224083
     Shore D ScaleD 224073
Calender Film: Opaque White (Pigmented with TiO2)
Specific GravityeD 7921.42
Tensile Strength @ Break 
     M.D.D 88247 MPa (6800 psi)
     T.D.D 88245 MPa (6500 psi)
Tensile Modulus, Tangent 
     M.D.D 8822050 MPa (3.0 x 105 psi)
     T.D.D 8822050 MPa (3.0 x 105 psi)
Tensile Modulus, 1% Secant 
     M.D.D 8822000 MPa (2.9 x 105 psi)
     T.D.D 8821950 MPa (2.9 x 105 psi)
Brittleness Temperature by ImpactdD 1790-40 °C (-40 °F)
Durometer Hardness 
     Shore A ScaleD 224086
     Shore D ScaleD 224074

aUnless noted otherwise, all tests are run at 23°C (73°F) and 50% relative humidity.
bUnless noted otherwise, the test method is ASTM.
cUnits are in SI or US customary units.
dData shown indicate test temperature at which all specimens break.
eDependent upon colorant, fillers, etc.



General
Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.


Eastman and its marketing affiliates shall not be responsible for the use of this information, or of any product, method, or apparatus mentioned, and you must make your own determination of its suitability and completeness for your own use, for the protection of the environment, and for the health and safety of your employees and purchasers of your products. No warranty is made of the merchantability of fitness of any product, and nothing herein waives any of the Seller's conditions of sale.